Download Solution PDFIdentify the type of casting defect indicated in the given diagram.
Answer (Detailed Solution Below)
Detailed Solution
Download Solution PDFExplanation:
Casting defects
Cold Shut
- A cold shut is caused when two streams while meeting in the mould cavity, do not fuse together properly thus forming a discontinuity in the casting.
- When the molten metal is poured into the mould cavity through a more-than-one gate, multiple liquid fronts will have to flow together and become one solid.
Misrun:
- When the molten metal solidifies before completely filling the mold cavity and leaves a space in the mold called as misrun.
- Cause:
- Low fluidity of the molten metal.
- Low temperature of the molten metal which decreases its fluidity.
- Too thin section and improper gating system.
- It is a void on the surface of the casting caused mainly due to uncontrolled and haphazard solidification of the metal.
- These are caused by the liquid shrinkage occurring during the solidification of the casting.
- To compensate this, proper feeding of liquid metal is required and also proper casting design.
- Shrinkage defects can be split into two different types:
- Open shrinkage defects
- Closed shrinkage defects
Last updated on Jul 18, 2025
-> DFCCIL Executive Answer Key 2025 has been released at its official website. Candidates can calculate their marks, estimate their scorecard with log in ID and Password.
-> The Objection window will remain open from 18th July to 22nd July 2025. Candidates can raise their objection with qid no. and proof.
-> The DFCCIL Rank Predictor 2025 is now available.
-> DFCCIL Executive Exam Analysis 2025 is live now. candidates can check level of exam, and estimate their score by analysing CBT 1 exam here.
-> DFCCIL Executive city intimation slip has been released.
-> DFCCIL Executive Recruitment 2025 Correction window is open from 31st March, to 4th April 2025.
-> Candidates can make corrections in their application form, if they have made any mistake. There will be 100/- fee for correction in form.
-> DFCCIL Executive Recruitment 2025 application deadline has been extended.
-> Eligible and Interested candidates had applied from 18th January 2025 to 22nd March 2025.
-> A total of 175 Vacancies have been announced for multiple posts like Executive (Civil, Electrical, Signal and Telecommunication).
-> Candidates who will get a successful selection under the DFCCIL Recruitment 2025 for the Executive selection process will get a salary range between Rs. 30,000 to Rs. 1,20,000.
-> Candidates must refer to the DFCCIL Executive Previous Year Papers to prepare well for the exam.